相关论文: Atomically Resolved Surface Structure of SrTiO3(00…
We have investigated the atomically-resolved substrate and homoepitaxial thin film surfaces of SrTiO3(001) using low-temperature scanning tunneling microscopy/spectroscopy (STM/STS) combined with pulsed laser deposition (PLD). It was found…
We report the growth of thin films of Sr1-xCaxRuO3 on SrTiO3 and MgO substrates by metalorganic aerosol deposition. The structure and microstructure is characterized by X-ray diffraction and room-temperature scanning tunnelling microscopy…
We have investigated the growth of BaTiO3 thin films deposited on pure and 1% Nb-doped SrTiO3(001) single crystals using atomic oxygen assisted molecular beam epitaxy (AO-MBE) and dedicated Ba and Ti Knudsen cells. Thicknesses up to 30 nm…
In this paper, we report the growth of NaxCoO2 thin films by pulsed-laser deposition (PLD). It is shown that the concentration of sodium is very sensitive to the substrate temperature and the target-substrate distance due to the evaporation…
Surfaces of homoepitaxially grown TiO2-terminated SrTiO3(001) were studied in situ with scanning tunneling microscopy and spectroscopy. By controlling the Ti/Sr ratio, two-dimensional domains of highly ordered linear nanostructures,…
We report on a systematic study of the growth of epitaxial TiO2 films deposited by pulsed laser deposition on Ti-terminated (001) SrTiO3 single crystals. By using in-situ reflection high energy electron diffraction, low energy electron…
The initial homoepitaxial growth of SrTiO3 on a (\surd13\times\surd13) - R33.7{\deg}SrTiO3(001) substrate surface, which can be prepared under oxide growth conditions, is atomically resolved by scanning tunneling microscopy. The identical…
Surface morphology of the substrate and bottom layers plays a critical role in the epitaxial growth of oxide thin films. Here, we report on the self-organized formation of a step-terrace structure in SrRuO3 (SRO) thin films grown using…
We report on growth-mode transitions in the growth of SrRuO3 thin films on atomically flat Ti4+ single-terminated SrTiO3 (111) substrates, investigated by reflection high-energy electron diffraction and atomic force microscopy. Over the…
High quality epitaxial thin-films of EuTiO3 have been grown on the (001) surface of SrTiO3 using pulsed laser deposition. In situ x-ray reflectivity measurements reveal that the growth is two-dimensional and enable real-time monitoring of…
The functional properties of devices based on perovskite oxides depend strongly on the growth modes that dramatically affect surface morphology and microstructure of the hetero-structured thin films. To achieve atomically flat surface…
An experimental study was conducted on controlling the growth mode of La0.7Sr0.3MnO3 thin films on SrTiO3 substrates using pulsed laser deposition (PLD) by tuning growth temperature, pressure and laser fluence. Different thin film…
Control of thin film stoichiometry is of primary relevance to achieve desired functionality. Pulsed laser deposition ablating from binary-oxide targets (sequential deposition) can be applied to precisely control the film composition,…
The availability of low-index rutile TiO2 single crystal substrates with atomically flat surfaces is essential for enabling epitaxial growth of rutile transition metal oxide films. The high surface energy of the rutile (001) surface often…
The recent emergence of topological insulators (TI) has spurred intensive efforts to grow TI thin films on various substrates. However, little is known about how robust the topological surface states (TSS) are against disorders and other…
Stoichiometric, epitaxial LaCrO3 films have been grown on TiO2-terminated SrTiO3(001) substrates by molecular beam epitaxy using O2 as the oxidant. Film growth occurred in a layer-by-layer fashion, giving rise to structurally excellent…
We use density functional theory (DFT) calculations to investigate structural models consisting of anatase TiO2(101) slabs covered by reduced overlayers formed by (101) crystallographic shear planes (CSPs). Ab initio thermodynamics supports…
We investigated the growth of titanium oxide two-dimensional (2D) nanostructures on Au(111), produced by Ti evaporation and post-deposition oxidation. Scanning tunneling microscopy and spectroscopy (STM and STS) and low-energy electron…
In a recent work by Ji Seop Oh et al., BaBiO3(001) thin films were grown on SrTiO3 by Pulsed Laser Deposition. It was argued that the films are BiO2-terminated from the modelling of angle-resolved photoemission spectroscopy experiments. The…
The (001)SrTiO3 crystal surface can be engineered to display a self-organized pattern of well-separated and nearly pure single-terminated SrO and TiO2 regions by high temperature annealing in oxidizing atmosphere. By using surface sensitive…