Abstract

We investigate Atomic Layer Deposition (ALD) of metal oxide on pristine and functionalized graphene. On pristine graphene, ALD coating can only actively grow on edges and defect sites, where dangling bonds or surface groups react with ALD precursors. This affords a simple method to decorate and probe single defect sites in graphene planes. We used perylene tetracarboxylic acid (PTCA) to functionalize graphene surface and selectively introduced densely packed surface groups on graphene. Uniform ultrathin ALD coating on PTCA graphene was achieved over large area. The functionalization method could be used to integrate ultrathin high-k dielectrics in future graphene electronics.

Keywords

Cite

@article{arxiv.0805.3712,
  title  = {Atomic Layer Deposition of Metal Oxides on Pristine and Functionalized Graphene},
  author = {Xinran Wang and Scott Tabakman and Hongjie Dai},
  journal= {arXiv preprint arXiv:0805.3712},
  year   = {2008}
}

Comments

6pages, 3 figures, J. Am. Chem. Soc. in press

R2 v1 2026-06-21T10:43:42.996Z