Atomic Layer Deposition Nucleation Dependence on Diamond Surface Termination

Materials Science 2023-07-20 v1 Quantum Physics

Abstract

Surface termination and interfacial interactions are critical for advanced solid-state quantum applications. In this paper, we demonstrate that atomic layer deposition (ALD) can both provide valuable insight on the chemical environment of the surface, having sufficient sensitivity to distinguish between the common diamond (001) surface termination types and passivate these interfaces as desired. We selected diamond substrates exhibiting both smooth and anomalously rough surfaces to probe the effect of morphology on ALD nucleation. We use high resolution in situ spectroscopic ellipsometry to monitor the surface reaction with sub-angstrom resolution, to evaluate the nucleation of an ALD Al2O3 process as a function of different ex and in situ treatments to the diamond surface. In situ water dosing and high vacuum annealing provided the most favorable environment for nucleation of dimethylaluminum isopropoxide and water ALD. Hydrogen termination passivated both smooth and rough surfaces while triacid cleaning passivated the smooth surface only, with striking effectiveness.

Keywords

Cite

@article{arxiv.2304.13834,
  title  = {Atomic Layer Deposition Nucleation Dependence on Diamond Surface Termination},
  author = {Jessica C. Jones and Nazar Delegan and F. Joseph Heremans and Alex B. F. Martinson},
  journal= {arXiv preprint arXiv:2304.13834},
  year   = {2023}
}

Comments

31 pages, 14 figures

R2 v1 2026-06-28T10:19:06.099Z