In the past decade, nanopores have been developed extensively for various potential applications, and their performance greatly depends on the surface properties of the nanopores. Atomic layer deposition (ALD) is a new technology for depositing thin films, which has been rapidly developed from a niche technology to an established method. ALD films can cover the surface in confined regions even in nano scale conformally, thus it is proved to be a powerful tool to modify the surface of the synthetic nanopores and also to fabricate complex nanopores. This review gives a brief introduction on nanopore synthesis and ALD fundamental knowledge, then focuses on the various aspects of synthetic nanopores processing by ALD and their applications, including single-molecule sensing, nanofluidic devices, nanostructure fabrication and other applications.
@article{arxiv.1309.5696,
title = {Surface Engineering of Synthetic Nanopores by Atomic Layer Deposition and Their Applications},
author = {Ceming Wang and Delin Kong and Qiang Chen and Jianming Xue},
journal= {arXiv preprint arXiv:1309.5696},
year = {2013}
}
Comments
11 pages, 12 figures, review paper, accepted by Frontiers of Materials Science