A Low-Temperature Atomic Layer Deposition Liftoff Method for Microelectronic and Nanoelectronic Applications

Mesoscale and Nanoscale Physics 2009-11-10 v2 Materials Science

Abstract

We report a novel method for depositing patterned dielectric layers with sub-micron features using atomic layer deposition (ALD). The patterned films are superior to sputtered or evaporated films in continuity, smoothness, conformality, and minimum feature size. Films were deposited at 100-150C using several different precursors and patterned using either PMMA or photoresist. The low deposition temperature permits uniform film growth without significant outgassing or hardbaking of resist layers. A liftoff technique presented here gives sharp step edges with edge roughness as low as ~10 nm. We also measure dielectric constants (k) and breakdown fields for the high-k materials aluminum oxide (k ~ 8-9), hafnium oxide (k ~ 16-19) and zirconium oxide (k ~ 20-29), grown under similar low temperature conditions.

Keywords

Cite

@article{arxiv.cond-mat/0305711,
  title  = {A Low-Temperature Atomic Layer Deposition Liftoff Method for Microelectronic and Nanoelectronic Applications},
  author = {M. J. Biercuk and D. J. Monsma and C. M. Marcus and J. S. Becker and R. G. Gordon},
  journal= {arXiv preprint arXiv:cond-mat/0305711},
  year   = {2009}
}

Comments

related papers available at http://marcuslab.harvard.edu

R2 v1 2026-07-22T10:50:43.546Z