中文

高纯铝和银中的纵向μ子自旋弛豫

材料科学 2015-05-27 v1

摘要

在室温下,利用时间微分μ子自旋弛豫技术,在纵向2 T磁场中测量了高纯铝和银样品中μ子自旋弛豫的时间依赖性。对于大于10 ns的时间,该形状很好地拟合为单指数函数,弛豫率分别为λAl=1.3±0.2(统计)±0.3(系统)\pms\lambda_{\textrm{Al}} = 1.3 \pm 0.2\,(\textrm{统计}) \pm 0.3\,(\textrm{系统})\,\pmsλAg=1.0±0.2(统计)±0.2(系统)\pms\lambda_{\textrm{Ag}} = 1.0 \pm 0.2\,(\textrm{统计}) \pm 0.2\,(\textrm{系统})\,\pms

关键词

引用

@article{arxiv.1102.4826,
  title  = {Longitudinal muon spin relaxation in high purity aluminum and silver},
  author = {J. F. Bueno and D. J. Arseneau and R. Bayes and J. H. Brewer and W. Faszer and M. D. Hasinoff and G. M. Marshall and E. L. Mathie and R. E. Mischke and G. D. Morris and K. Olchanski and V. Selivanov and R. Tacik},
  journal= {arXiv preprint arXiv:1102.4826},
  year   = {2015}
}