We have measured the quantum-interference magnetoresistances in two single indium tin oxide (ITO) nanowires between 0.25 and 40 K, by using the four-probe configuration method. The magnetoresistances are compared with the one-dimensional weak-(anti)localization theory to extract the electron dephasing length LϕL_\phi. We found, in a 60-nm diameter nanowire with a low resistivity of ρ\rho(10 K) = 185 μΩ\mu \Omega cm, that LϕL_\phi is long, increasing from 150 nm at 40 K to 520 nm at 0.25 K. Therefore, the nanowire reveals strict one-dimensional weak-localization effect up to several tens of degrees of Kelvin. In a second 72-nm diameter nanowire with a high resistivity of ρ\rho(10 K) = 1030 μΩ\mu \Omega cm, the dephasing length is suppressed to LϕL_\phi(0.26 K) = 200 nm, and thus a crossover of the effective device dimensionality from one to three occurs at about 12 K. In particular, disorder-induced spin-orbit coupling is evident in the latter sample, manifesting weak-antilocalization effect at temperatures below \sim 4 K. These observations demonstrate that versatile quantum-interference effects can be realized in ITO nanowires by controlling differing levels of atomic defects and impurities.

Keywords

Cite

@article{arxiv.1010.5863,
  title  = {Long electron dephasing length and disorder-induced spin-orbit coupling in indium tin oxide nanowires},
  author = {Yao-Wen Hsu and Shao-Pin Chiu and An-Shao Lien and Juhn-Jong Lin},
  journal= {arXiv preprint arXiv:1010.5863},
  year   = {2010}
}

Comments

Phys. Rev. B (accepted)