Related papers: High-Resolution Thermal Expansion of MgB2
The thermoelectric transport properties of CaMg2Bi2, EuMg2Bi2, and YbMg2Bi2 were characterized between 2 and 650K. As synthesized, the polycrystalline samples are found to have lower p-type carrier concentrations than single-crystalline…
This review paper illustrates the main normal and superconducting state properties of magnesium diboride, a material known since early 1950's, but recently discovered to be superconductive at a remarkably high critical temperature Tc=40K…
The specific heat $C(T)$ of BaFe$_2$As$_2$ single crystal, electron-doped Ba$_{0.7}$La$_{0.3}$Fe$_2$As$_2$ and hole-doped Ba$_{0.5}$K$_{0.5}$Fe$_2$As$_2$ polycrystals were measured. For undoped BaFe$_2$As$_2$ single crystal, a very sharp…
Lattice parameter of metastable high-pressure phase of zinc oxide, rock-salt ZnO was measured in the 10-300 K temperature range using synchrotron X-ray powder diffraction. No phase transition was observed down to 10 K. The lattice parameter…
The real $R_s(T)$ and imaginary $X_s(T)$ parts of the surface impedance $Z_s(T)=R_s(T)+iX_s(T)$ in polycrystalline MgB$_2$ samples of different density with the critical temperature $T_c\approx 38$ K are measured at the frequency of 9.4 GHz…
The upper critical field Hc2(T) of sintered pellets of the recently discovered MgB_2 superconductor was investigated by transport, ac susceptibility and dc magnetization measurements in magnetic fields up to 16 T covering a temperature…
The temperature dependence of the London penetration depth, $\lambda(T)$, was measured in polycrystalline MgB$_2$ samples by a high-resolution, radio frequency technique. A clear exponential temperature dependence of $\lambda(T)$ was…
Bulk single crystals of manganese phosphide (MnP) were grown from melt at 1 GPa and 1200 C by using a cubic-anvil, high-pressure, and high-temperature technique. The obtained black colored crystals exhibit a plate-like morphology, with flat…
We report the synthesis and measurements of magnetic, transport, and thermal properties of polycrystalline Nb0.18Re0.82, which has a superconducting transition at Tc ~ 8.8 K. The non-centrosymmetric alpha-Mn structure of the compound is…
Infrared absorption measurements in the range of 125 to 700 cm^(-1) have been carried out as a function of temperature upto 5 K in MgB2. The absorption spectrum is characterised by a broad band centred at 485 cm^{-1}, with shoulders at 333…
We investigate the effects of carbon and boron doping on the thermal expansion in the hexagonal (P63/mmc) intermetallic YbGaGe. X-ray powder diffraction was used to measure the lattice constants on pure and doped (C or B at nominal levels…
We report the effect of the sintering temperature on the superconductivity of MgB2 pellets prepared under a high pressure of 3 GPa. The superconducting properties of the non-heated MgB2 in this high pressure were poor. However, as the…
The thermal expansion coefficients of $\mathrm{Na}_{N}$ clusters with $8 \le N \le 40$ and $\mathrm{Al}_{7}$, $\mathrm{Al}_{13}^-$ and $\mathrm{Al}_{14}^-$ are obtained from {\it ab initio} Born-Oppenheimer LDA molecular dynamics. Thermal…
We report a new design of temperature-modulated dilatometer, which obtains the linear thermal expansion coefficient by measuring the oscillating changes of the sample's length and temperature by a piezobender and a thermocouple,…
The two-gap structure in the superconducting state of MgB_2 gives rise to unusual thermodynamic properties which depart markedly from the isotropic single-band BCS model, both in their temperature- and field dependence. We report and…
The specific heat C of a sintered polycrystalline sample of MgB2 with a bulk superconducting transition temperature Tc=36.7 K is measured as a function of the temperature (2-300 K) and magnetic field (0-16 T), together with magnetic…
Bulk single crystals of manganese arsenide (MnAs) were grown from melt at 1 GPa and 1100 {\deg}C by using a cubic-anvil, high-pressure, and high-temperature technique. The as-grown black colored crystals extracted from solidified lump…
The temperature and pressure dependent electrical resistivity rho(T,P) studies have been performed on BaMn2As2 single crystal in the 4.2 to 300 K range upto of 8.2 GPa to investigate the evolution of its ground state properties. The rho(T)…
A novel approach based on dynamic thermal vibration is proposed to calculate the heat capacity and thermal expansion coefficient (TEC) for metal crystalline materials from 0K to the melting point. The motion of metal atomic clusters is…
We present thermal expansion and longitudinal magnetostriction data for cubic RAl3 (R = Tm, Yb, Lu) single crystals. The thermal expansion coefficient for YbAl3 is consistent with an intermediate valence of the Yb ion, whereas the data for…