Related papers: Spectacular decrease of the melting magnetic field…
Epitaxial LaRh1/2Mn1/2O3 thin films have been grown on (001)-oriented LaAlO3 and SrTiO3 substrates using pulsed laser deposition. The optimized thin film samples are semiconducting and ferromagnetic with a Curie temperature close to 100 K,…
Epitaxial thin films of La0.7Ba0.3MnO3 manganite, deposited using Chemical Solution Deposition technique, were irradiated by 200 MeV Ag+15 ions with a maximum ion dose up to 1x10^12 ions/cm2. Temperature- and magnetic field-dependent…
FeSe0.5Te0.5 thin films with PbO-type structure are successfully grown on MgO(100) and LaSrAlO4(001) substrates from FeSe0.5Te0.5 or FeSe0.5Te0.75 polycrystalline targets by pulsed-laser deposition. The film deposited on the MgO substrate…
We present electric and magnetic properties of 0.8Pb(Fe1/2Nb1/2)O3-0.2Pb(Mg1/2W1/2)O3 films epitaxially grown on (001) SrTiO3 substrates using pulsed laser deposition. A narrow deposition window around 710 oC and 0.2 mbar has been…
Superconducting thin films of MgB2 were deposited by Pulsed Laser Deposition on magnesium oxide and sapphire substrates. Samples grown at 450C in an argon buffer pressure of about 10-2 mbar by using a magnesium enriched target resulted to…
We report on the magnetic properties of zinc ferrite thin film deposited on SrTiO$_3$ single crystal using pulsed laser deposition. X-ray diffraction result indicates the highly oriented single phase growth of the film along with the…
Al-doped ZnO thin films were deposited using reactive high power impulse magnetron sputtering at substrate temperatures between room temperature and 600 $\bullet$ C. Two sample series with different oxygen partial pressures were studied.…
5$\mu$m thick SmCo films were deposited onto Si substrates using triode sputtering. A study of the influence of deposition temperature (Tdep <= 600 degrees C) on the structural, magnetic and mechanical properties has shown that optimum…
V2O3 thin films about 10 nm thick were grown on Al2O3 (0001) by pulsed laser deposition. The XRD analysis is in agreement with R-3c space group. Some of them exhibit the metal / insulator transition characteristic of V2O3 bulk material and…
We present a comprehensive study of the thickness dependence of static and magneto-dynamic magnetic properties of La$_{0.7}$Sr$_{0.3}$MnO$_3$. Epitaxial pulsed laser deposited La$_{0.7}$Sr$_{0.3}$MnO$_3$ / SrTiO$_3$(001) thin films in the…
We report the growth of high-quality c-axis-oriented epitaxial MgB2 thin films by using a pulsed laser deposition technique. The thin films grown on (1`1 0 2) Al2O3 substrates show a Tc of 39 K. The critical current density in zero field is…
Simultaneous studies on the magnetic and electrotransport properties of Nd_{0.67} Sr_{0.33} Mn_{1-x} Fe_x O_3 polycrystalline bulk and epitaxial thin films (x = 0.00 and 0.05) have been carried out. A magnetoresistance (MR) as high as ~ 33%…
We present a study of the synthesis of epitaxial V$_2$O$_3$ films on $c$-plane Al$_2$O$_3$ substrates by reactive dc-magnetron sputtering. The results reveal a temperature window, at substantially lower values than previously reported,…
We observe an unusual behavior of the spin Hall magnetoresistance (SMR) measured in a Pt ultra-thin film deposited on a ferromagnetic insulator, which is a tensile-strained LaCoO3 (LCO) thin film with the Curie temperature Tc=85K. The SMR…
We report the magnetoresistance and nonlinear Hall effect studies over a wide temperature range in pulsed laser deposited Ni0.07Zn0.93O thin film. Negative and positive contributions to magnetoresistance at high and low temperatures have…
High-quality thin films of the ferromagnetic-insulator europium(II) sulfide (EuS) were fabricated by pulsed laser deposition on Al2O3 (0001) and Si (100) substrates. A single orientation was obtained with the [100] planes parallel to the…
The structural, magnetic and dielectric properties have been investigated in 3$d$-5$d$ based double perovskite Sr$_2$FeIrO$_6$ thin films deposited by pulse laser deposition technique. To understand the effect of strain, epitaxial films are…
We measured the temperature dependence of the saturation magnetization (Ms) of a (La1-xPrx)1-yCayMnO3 (x ~ 0.60, y ~ 0.33) film as a function of applied bending stress. Stress producing a compressive strain of -0.01% along the magnetic easy…
The effect of annealing under a magnetic field on the microstructure and properties of YNixMn1-xO3 (x=0.33 and 0.5) films has been investigated. It is found that the ferromagnetic transition temperature is significantly enhanced after post…
A series of MgB2 thin films were fabricated by pulsed laser deposition (PLD), doped with various amounts of Si up to a level of 18wt%. Si was introduced into the PLD MgB2 films by sequential ablation of a stoichiometric MgB2 target and a Si…