Surface Diffusion Control Enables Tailored Aspect Ratio Nanostructures in Area-Selective Atomic Layer Deposition

Materials Science 2020-12-09 v1

Abstract

Area-selective atomic layer deposition is a key technology for modern microelectronics as it eliminates alignment errors inherent to conventional approaches by enabling material deposition only in specific areas. Typically, the selectivity originates from surface modifications of the substrate that allow or block precursor adsorption. The control of the deposition process currently remains a major challenge as the selectivity of the no-growth areas is lost quickly. Here, we show that surface modifications of the substrate strongly manipulate the surface diffusion. The selective deposition of TiO2_2 on poly (methyl methacrylate) and SiO2_2 yields localized nanostructures with tailored aspect ratios. Controlling the surface diffusion allows to tune such nanostructures as it boosts the growth rate at the interface of the growth and no-growth areas. Kinetic Monte-Carlo calculations reveal that species move from high to low diffusion areas. Further, we identify the catalytic activity of TiCl4_4 during the formation of carboxylic acid on poly (methyl methacrylate) as the reaction mechanism responsible for the loss of selectivity, and show that process optimization leads to higher selectivity. Our work enables the precise control of area-selective atomic layer deposition on the nanoscale, and offers new strategies in area-selective deposition processes by exploiting surface diffusion effects.

Keywords

Cite

@article{arxiv.2012.04465,
  title  = {Surface Diffusion Control Enables Tailored Aspect Ratio Nanostructures in Area-Selective Atomic Layer Deposition},
  author = {Philip Klement and Daniel Anders and Lukas Gümbel and Michele Bastianello and Fabian Michel and Jörg Schörmann and Matthias T. Elm and Christian Heiliger and Sangam Chatterjee},
  journal= {arXiv preprint arXiv:2012.04465},
  year   = {2020}
}

Comments

24 pages, 11 figures, including supporting material

R2 v1 2026-06-23T20:48:59.299Z