Atomic layer deposition of titanium nitride for quantum circuits

Mesoscale and Nanoscale Physics 2018-12-05 v2 Applied Physics Quantum Physics

Abstract

Superconducting thin films with high intrinsic kinetic inductance are of great importance for photon detectors, achieving strong coupling in hybrid systems, and protected qubits. We report on the performance of titanium nitride resonators, patterned on thin films (9-110 nm) grown by atomic layer deposition, with sheet inductances of up to 234 pH/square. For films thicker than 14 nm, quality factors measured in the quantum regime range from 0.4 to 1.0 million and are likely limited by dielectric two-level systems. Additionally, we show characteristic impedances up to 28 kOhm, with no significant degradation of the internal quality factor as the impedance increases. These high impedances correspond to an increased single photon coupling strength of 24 times compared to a 50 Ohm resonator, transformative for hybrid quantum systems and quantum sensing.

Keywords

Cite

@article{arxiv.1808.06009,
  title  = {Atomic layer deposition of titanium nitride for quantum circuits},
  author = {A. Shearrow and G. Koolstra and S. J. Whiteley and N. Earnest and P. S. Barry and F. J. Heremans and D. D. Awschalom and E. Shirokoff and D. I. Schuster},
  journal= {arXiv preprint arXiv:1808.06009},
  year   = {2018}
}

Comments

10 pages, 8 figures including supplemental materials

R2 v1 2026-06-23T03:37:14.594Z