Quenched-Vacancy Induced Spin-Glass Order
Abstract
The ferromagnetic phase of an Ising model in d=3, with any amount of quenched antiferromagnetic bond randomness, is shown to undergo a transition to a spin-glass phase under sufficient quenched bond dilution. This general result, demonstrated here with the numerically exact renormalization-group solution of a d=3 hierarchical lattice, is expected to hold true generally, for the cubic lattice and for quenched site dilution. Conversely, in the ferromagnetic-spinglass-antiferromagnetic phase diagram, the spin-glass phase expands under quenched dilution at the expense of the ferromagnetic and antiferromagnetic phases. In the ferro-spinglass phase transition induced by quenched dilution reentrance is seen, as previously found for the ferro-spinglass transition induced by increasing the antiferromagnetic bond concentration.
Cite
@article{arxiv.0811.0025,
title = {Quenched-Vacancy Induced Spin-Glass Order},
author = {Gül Gülpınar and A. Nihat Berker},
journal= {arXiv preprint arXiv:0811.0025},
year = {2009}
}
Comments
Added data, references. 4 pages, 4 figures. Published version