Related papers: Superconductivity in Polycrystalline Diamond Thin …
Diamond has always been adored as a jewel. Even more fascinating is its outstanding physical properties; it is the hardest material known in the world with the highest thermal conductivity. Meanwhile, when we turn to its electrical…
The superconductivity transition temperatures Tc(onset) of 11.4 K and Tc(offset) of 7.4 K, which are the highest in diamond at present, are realized on homoepitaxially grown (111) diamond films with a high boron doping concentration of…
Boron-doped diamond granular thin films are known to exhibit superconductivity with an optimal critical temperature of Tc = 7.2K. Here we report the measured complex surface impedance of Boron-doped diamond films in the microwave frequency…
Diamond has outstanding physical properties: the hardest known material, a wide band gap, the highest thermal conductivity, and a very high Debye temperature. In 2004, Ekimov et al. discovered that heavily boron-doped (B-doped) diamond…
We report the discovery of superconductivity in boron-doped diamond synthesized at high pressure (8-9 GPa) and temperature (2,500-2,800 K). Electrical resistivity, magnetic susceptibility, specific heat, and field-dependent resistance…
Homoepitaxial diamond layers doped with boron in the 10^20-10^21 /cm3 range are shown to be type II superconductors with sharp transitions (~0.2K) at temperatures increasing from 0 to 2.1 K with boron contents. The critical concentration…
Heavily-boron-doped diamond films become superconducting with critical temperatures $T_c$ well above 4 K. Here we first measure the reflectivity of such a film down to 5 cm$^{-1}$, by also using Coherent Synchrotron Radiation. We thus…
Superconducting thin films have been prepared on Si-substrates, using pulsed laser deposition from a target composed of a mixture of Mg and MgB2 powders. The films were deposited at room temperature and post-annealed at 600 degrees C. The…
Superconducting MgB(2) films with Tc = 38.6 K were prepared using a precursor-deposition, ex-situ post-processing approach. Precursor films of boron, ~0.5 micrometer thick, were deposited onto Al(2)O(3) (102) substrates by e-beam…
Thin films of MgB2 superconductor were prepared by three different procedures on sapphire and silicon substrates. Boron thin films, ex-situ annealed in magnesium vapour, resulted in textured polycrystalline films with crystal dimensions…
The boron-doped single crystal diamond films were grown homoepitaxially on synthetic (100) oriented Type Ib diamond substrates using a Microwave Plasma Chemical Vapor Deposition (MPCVD) technique. Raman spectrum showed a few additional…
We have investigated the low energy electronic state of a boron-doped diamond thin film by the ultrahigh resolution laser-excited photoemission spectroscopy. We observed a clear shift of the leading edge below 11 K indicative of a…
We report on the transport properties of nanostructures made from boron-doped superconducting diamond. Starting from nanocrystalline superconducting boron-doped diamond thin films, grown by Chemical Vapor Deposition, we pattern by…
Superconducting MgB2 thin films were prepared on Al2O3(0001) and MgO(100) substrates. Boron thin films were deposited by the electron-beam evaporation followed by post-annealing process with magnesium. Proper post annealing conditions were…
Single-crystalline diamond (SCD) films possess exceptional thermal, chemical, and optical properties, making them ideal for advanced applications. However, achieving uniform film quality via microwave plasma chemical vapor deposition…
Microwave plasma chemical vapor deposition (MPCVD) has been traditionally used to synthesize carbon-based materials such as diamonds, carbon nanotubes and graphene. Here we report that a rapid and catalyst-free growth of SnSe thin films can…
Scanning tunneling spectroscopies are performed below 100~mK on nano-crystalline boron-doped diamond films characterized by Transmission Electron Microscopy and transport measurements. We demonstrate a strong correlation between the local…
Superconducting thin films of MgB2 were deposited by Pulsed Laser Deposition on magnesium oxide and sapphire substrates. Samples grown at 450C in an argon buffer pressure of about 10-2 mbar by using a magnesium enriched target resulted to…
We report the experimental discovery of superconductivity with critical temperature Tc above 70 K in zirconium polyhydrides, the record high so far for 3d transition metal hydrides. The superconducting zirconium polyhydrides are synthesized…
Superconducting MgB2 thin films were fabricated on Al2O3(0001) substrates under an ex-situ processing conditions. Boron thin films were deposited by pulsed laser deposition followed by a post-annealing process. Resistance measurements of…