Related papers: Pure phase BiFeO$_3$ thin films sputtered over Si:…
Multiferroic BiFeO3 (BFO) thin film exhibiting desired ferroelectric and enhanced magnetic properties was grown on La0.67Sr0.33MnO3 (LSMO) buffered Pt/TiO2/SiO2/Si substrates by off-axis RF magnetic sputtering, where a highly (111)-oriented…
Single phase (001)-oriented BiFeO3 (BFO) thin films grown by pulsed laser deposition can only be obtained in a narrow window of deposition pressure and temperature and have a low magnetic moment. Out of the stability window Fe- or Bi-rich…
Epitaxial Mn-doped BiFeO3 (MBFO) thin films were grown on GaAs (001) substrate with SrTiO3 (STO) buffer layer by pulsed laser deposition. X-ray diffraction results demonstrate that the films show pure (00l) orientation, and…
Multiferroic BiFeO3 (BFO) / La0.7Sr0.3MnO3 heterostructured thin films were grown by pulsed laser deposition on polished spark plasma sintered LaAlO3 (LAO) polycrystalline substrates. Both polycrystalline LAO substrates and BFO films were…
A previous study of the growth conditions has shown that single-phase BiFeO3 thin films can only be obtained in a narrow pressure-temperature window and that these films display a weak magnetic moment. Here we study in more detail the…
The magnetic domain structure of the multiferroic Bi1-xDyxFeO3 (BDFO) deposited on ZnO at the macroscopic level has been demonstrated in this paper. Magnetic properties are observed by saturated magnetic and ferroelectric hysteresis loops…
Multiferroic BiFeO$_3$ (BFO) possesses a rich phase diagram that allows strain tuning of its properties in thin-film form. In particular, at large compressive strain, a supertetragonal (T) phase with giant polarization is stabilized over…
The properties of epitaxial Bi2FeCrO6 thin films, recently synthesized by pulsed laser deposition, have partially confirmed the theoretical predictions (i.e. a magnetic moment of 2 muB per formula unit and a polarization of ~80 microC/cm2…
BiFeO$_3$ (BFO) shows both ferroelectricity and magnetic ordering at room temperature but its ferromagnetic component, which is due to spin canting, is negligible. Substitution of transition-metal atoms such as Co for Fe is known to enhance…
Room-temperature magnetoelectric multiferroicity has been observed in c-axis oriented GaFeO$_3$ thin films (space group $Pna2_1$), grown on economic and technologically important (100)Si substrates by pulsed laser deposition technique.…
The influence of the deposition pressure PO2 and substrate temperature TS during the growth of Bi2FeCrO6 thin films grown by pulsed laser deposition has been investigated. It is found that the high volatility of Bi makes the deposition very…
SrFe$_{12}$O$_{19}$ (SFO) films grown on Si (100) substrates by radio-frequency magnetron sputtering have been characterized in terms of composition, structural and magnetic properties by a combination of microscopy, diffraction and…
We report the epitaxial growth of BiFeO3 by pulsed electron deposition and the resulting crystal quality, magnetic and nanoscale switching properties. X-ray diffraction shows high quality single phase, epitaxial (001) oriented films grown…
Thin films of (1-x)BiFeO<sub>3</sub>-xPbTiO<sub>3</sub> (BF-xPT) with x ~ 0.60 were fabricated on Pt/Si substrates by chemical solution deposition of precursor BF and PT layers alternately in three different multilayer configurations. These…
NiFe$_2$O$_4$ thin films with varying thickness were grown on SrTiO$_3$(001) by reactive molecular beam epitaxy. Soft and hard x-ray photoelectron spectroscopy measurements reveal a homogeneous cation distribution throughout the whole film…
Recent works have shown that the domain walls of room-temperature multiferroic BiFeO3 (BFO) thin films can display distinct and promising functionalities. It is thus important to understand the mechanisms underlying domain formation in…
We report the structural and physical properties of epitaxial Bi2FeCrO6 thin films on epitaxial SrRuO3 grown on (100)-oriented SrTiO3 substrates by pulsed laser ablation. The 300 nm thick films exhibit both ferroelectricity and magnetism at…
We have explored the influence of deposition pressure and temperature on the growth of BiFeO3 thin films by pulsed laser deposition onto (001)-oriented SrTiO3 substrates. Single-phase BiFeO3 films are obtained in a region close to 10-2 mbar…
We report a study on the thermodynamic stability and structure analysis of the epitaxial BiFeO3 (BFO) thin films grown on YAlO3 (YAO) substrate. First we observe a phase transition of MC-MA-T occurs in thin sample (<60 nm) with an utter…
We grew a 2 micron thick film of single-phase BiFeO3 on a Si (100) substrate by pulsed laser deposition with a substrate temperature of 575 oC and an oxygen partial pressure of 0.06 mbar. X ray diffraction analysis indicated that the film…