Related papers: Large Thermoelectric Power Factor at Low Temperatu…
We found that whisker crystals of Mo-doped Nb4SiTe4 show high thermoelectric performances at low temperatures, indicated by the largest power factor of 70 microW cm-1 K-2 at 230-300 K, much larger than those of Bi2Te3-based practical…
One-dimensional tellurides Ta4SiTe4 and Nb4SiTe4 were found to show high thermoelectric performance below room temperature. This study reported the synthesis and thermoelectric properties of whisker crystals of Ta4SiTe4-Nb4SiTe4 solid…
A TiS$_{2}$ crystal with a layered structure was found to have a large thermoelectric power factor.The in-plane power factor $S^{2}/ \rho$ at 300 K is 37.1~$\mu$W/K$^{2}$cm with resistivity ($\rho$) of 1.7 m$\Omega$cm and thermopower ($S$)…
Solid-state thermoelectric cooling is expected to be widely used in various cryogenic applications such as local cooling of superconducting devices. At present, however, thermoelectric cooling using p- and n-type Bi2Te3-based materials has…
Ta4SiTe4 is a one-dimensional van der Waals material that exhibits an exceptionally large thermoelectric power factor below room temperature. However, since this material has been available only in the form of acicular microcrystals,…
We have measured thermoelectric properties of Ta2PdX6 (X=S, Se) around room temperature using single crystal samples. We find that the power factor of Ta2PdX6 is relatively high from middle-low to room temperatures, and notably Ta2PdSe6…
The thermoelectric and transport properties of a Fe3O4/SiO2/p-Si(100) heterostructure have been investigated between 100 and 300 K. Both Hall and Seebeck coefficients change sign from negative to positive with increasing temperature while…
In the past decade, there has been significant interest in the potentially advantageous thermoelectric properties of one-dimensional (1D) nanowires, but it has been challenging to find high thermoelectric power factors based on 1D effect in…
Polycrystalline samples of Er$_{1-x}$Ho$_x$NiSb ($x$ = 0, 0.2, 0.3, 0.5, 0.7, 0.8, 1) were characterized by means of x-ray powder diffraction (XRD), scanning electron microscopy (SEM), and optical metallography. The results proved the…
We found that a high mobility semimetal 1T'-MoTe2 shows a significant pressure-dependent change in the cryogenic thermopower in the vicinity of the critical pressure, where the polar structural transition disappears. With the application of…
Results of the measurements of thermoelectric properties of thin semiconductor microwires of Pb1-xTlxTe (x=0,001-0,02, d=5-100mkm) in the temperature region 4,2-300 K, which were obtained from solution melt by the filling of the quartz…
Thermoelectric (TE) materials are useful for applications such as waste heat harvesting or efficient and targeted cooling. While various strategies towards superior thermoelectrics through a reduction of the lattice thermal conductivity…
We investigated the optical properties of single crystals of one-dimensional telluride Ta4SiTe4, which shows high thermoelectric performance below room temperature. Optical conductivity estimated from reflectivity spectra indicates the…
Thermoelectric properties of polycrystalline p-type ZrTe5 are reported in temperature (T) range 2 - 340 K. Thermoelectric power (S) is positive and reaches up to 458 uV/K at 340 K on increasing T. The value of Fermi energy 16 meV, suggests…
Single-crystalline silicon is well known to be a poor thermoelectric material due to its high thermal conductivity. Most excellent research has focused on ways to decrease its thermal conductivity while retaining acceptably large power…
We report results of ultrasonic studies of a single crystal of KDP in the temperature range 2-300 K. The longitudinal and transverse sound velocities along [001] and [100] directions were obtained as functions of temperature. The analysis…
The Hall and Seebeck coefficients, electrical resistivity and thermal conductivity of polycrystalline NiSi3P4 were characterized from 2 to 775K. Undoped NiSi3P4 behaves like a narrow gap semiconductor, with activated electrical resistivity…
Here we report a record thermoelectric power factor of up to 160 $\mu$ W m-1 K-2 for the conjugated polymer poly(3-hexylthiophene) (P3HT). This result is achieved through the combination of high-temperature rubbing of thin films together…
We have measured the electrical resistivity ($\rho$) and the thermoelectric power (TEP) of the perchlorate (ClO4^-) doped stretch oriented polyacetylene (PA) film. For the highly conducting samples ($\sigma_{RT} > 41000 S/cm$), the…
The potential of bulk black-phosphorus for thermoelectric applications has been experimentally studied. The Seebeck Coefficient (S) has been measured in the temperature range from 300 K to 385 K, finding a value of S = +335 +- 10 uV/K at…