We report a study on the thermodynamic stability and structure analysis of the epitaxial BiFeO3 (BFO) thin films grown on YAlO3 (YAO) substrate. First we observe a phase transition of MC-MA-T occurs in thin sample (<60 nm) with an utter…
Multiferroic materials attract considerable interest because of the wide range of potential applications such as spintronic devices, data storage and sensors. As a strong candidate for the applications among the limited list of single-phase…
We report visible light detection with in-plane BiFeO3 (BFO) thin films grown on pre-patterned inter-digital electrodes. In-plane configured BFO film displayed photocurrents with a 40:1 photo-to-dark-current ratio and improved photo-sensing…
Fatigue failure in ferroelectrics has been intensively investigated in the past few decades. Most of the mechanisms discussed for ferroelectric fatigue have been built on the "hypothesis of variation in charged defects", which however are…
We grew a 2 micron thick film of single-phase BiFeO3 on a Si (100) substrate by pulsed laser deposition with a substrate temperature of 575 oC and an oxygen partial pressure of 0.06 mbar. X ray diffraction analysis indicated that the film…
We investigated the electronic and magnetic properties of fully oxidized BaFeO3 thin films, which show ferromagnetic-insulating properties with cubic crystal structure, by hard x-ray photoemission spectroscopy (HAXPES), x-ray absorption…
The temperature dependence of the relaxation dynamics in the bilayer thin film heterostructure composed of multiferroic BiFeO$_{3}$ (BFO) and superconducting YBa$_{2}$Cu$_{3}$O$_{7}$ (YBCO) grown on a (001) SrTiO$_{3}$ substrate is studied…
In-plane temperature dependent dielectric behavior of BiFeO3 (BFO) as-grown thin films show diffuse but prominent phase transitions near 450 (+/-10) K and 550 K with dielectric loss temperature dependences that suggest skin layer effects.…
We present the temperature- and thickness-dependent structural and morphological evolution of strain induced transformations in highly-strained epitaxial BiFeO3 films deposited on LaAlO3 (001) substrates. Using high-resolution X-ray…
Multiferroic BiFeO3 epitaxial films with thickness ranging from 40 nm to 960 nm were grown by pulsed laser deposition on SrTiO3 (001) substrates with SrRuO3 bottom electrodes. X-ray characterization shows that the structure evolves from…
Sm0.53Sr0.47MnO3 thin films were deposited on single crystal LaAlO3 (LAO/(001)) and SrTiO3 (STO/(001)) substrates by DC magnetron sputtering. The theta-2theta and omega-2theta scans show that these films have very good crystallinity and the…
Thin films of (1-x)BiFeO<sub>3</sub>-xPbTiO<sub>3</sub> (BF-xPT) with x ~ 0.60 were fabricated on Pt/Si substrates by chemical solution deposition of precursor BF and PT layers alternately in three different multilayer configurations. These…
Epitaxial 200nm BiFe$_{0.95}$Mn$_{0.05}$O$_{3}$ (BFO) film was grown by pulsed laser deposition on (111) oriented SrTiO3 substrate buffered with a 50nm thick SrRuO$_{3}$ electrode. The BFO thin film shows a rhombohedral structure and a…
Multiferroic BiFeO$_3$ (BFO) possesses a rich phase diagram that allows strain tuning of its properties in thin-film form. In particular, at large compressive strain, a supertetragonal (T) phase with giant polarization is stabilized over…
Exchange biased Ni/ FeF2 films have been investigated using vector coil vibrating sample magnetometry as a function of the cooling field strength H_FC. In films with epitaxial FeF2, a loop bifurcation develops with increasing H_FC as it…
Post deposition variation in film resistance of Sb2Te3 films deposited on glass substrates at room temperature and an elevated temperature (110oC) are investigated. The resistance of films grown at room temperature shows a non-linear…
Bismuth ferrite (BiFeO3) is one of the rare materials that exhibits multiferroic properties already at room-temperature. Therefore, it offers tremendous potential for future technological applications, such as memory and logic. However, a…
BiFeO3 thin films have been grown on Pt/Ti/SiO2/Si substrates with pulsed laser deposition using Au as the top electrode. The resistive switching property of the Au/BiFeO3/Pt stack has been significantly improved by carefully tuning the…
A remarkably high saturation magnetization of ~0.4mu_B/Fe along with room temperature ferromagnetic hysteresis loop has been observed in nanoscale (4-40 nm) multiferroic BiFeO_3 which in bulk form exhibits weak magnetization (~0.02mu_B/Fe)…
The magnetic domain structure of the multiferroic Bi1-xDyxFeO3 (BDFO) deposited on ZnO at the macroscopic level has been demonstrated in this paper. Magnetic properties are observed by saturated magnetic and ferroelectric hysteresis loops…