Related papers: Highly luminescent a-SiOx<Er>/SiO2/Si multilayer s…
We present a resonant approach to enhance 1550nm emission efficiency of amorphous silicon sub-oxide doped with Er3+ (a-SiOx<Er>) layers with silicon nanoclusters (Si-NC). Two distinct techniques were combined to provide a structure that…
The enhancement of Er$^{3+}$-based up-conversion for photovoltaics in multilayer porous silicon photonic structures is considered theoretically and experimentally. Transfer matrix simulations are used to assess the increased photonic…
The study of hexagonal silicon polytypes attracts special attention due to their unique physical properties compared to the traditional cubic phase of Si. Thus, for some hexagonal phases, a significant improvement in the emission properties…
A relationship between the chemical composition, structure and luminescent properties of light-emitting SiOxNy(Si) composite layers with Si nanocrystals is demonstrated. Photoluminescence (PL) with a maximum of intensity at 500-600 nm is…
Prior studies have shown that photoluminescence from Er3+ impurities in silicon is severely limited at room temperature by non-radiative relaxation and solid solubility; and room temperature emission from Er3+ in oxide-based hosts becomes…
We report a significant enhancement of room-temperature photoluminescence from trivalent erbium-doped (Er3+) silicon nitride (Si3N4) metasurfaces at the telecommunication wavelength prepared via ion implantation. The metasurfaces,…
The silicon suboxide SiOx (x<2.0) offers promising industrial application possibilities ranging from electrodes in lithium-ion batteries, which are used widely in electrical vehicles and portable devices to sensing applications. Therefore,…
The demand for single photon sources at $\lambda~=~1.54~\mu$m, which follows from the consistent development of quantum networks based on commercial optical fibers, makes Er:O$_x$ centers in Si still a viable resource thanks to the optical…
Samples of amorphous MgSiO_3 annealed at temperature steps leading up to their crystallisation temperature show a rise in photoluminescence activity, peaking at ~450C. The photoluminescence band has a main peak at 595nm and a weaker peak at…
We have studied the 1.5 $\mu$m photoluminescence (PL) from Er ions after annealing two different sample sets in the temperature range 500 °C to 1100 °C. The different sample sets were made by magnetron sputtering from composite…
The broadening and optical parameters of TiO2/SiO2 transition layers depending on the ion energy have been investigated using the Rutherford Backscattering Spectrometry (RBS) and Ellipstrometry Spectroscopy (ES) methods. The TiO2/SiO2…
Silicon (Si) nanoparticles (NPs) were synthesized by transforming Si wafer surface to ammonium silicon hexafluoride (ASH) or (NH4)2SiF6 under acid vapor treatment. Si-NPs are embedded within the polycrystalline (ASH) layer formed on the Si…
Erbium implanted silicon (Er:Si) is a promising platform for quantum networking applications, but a major obstacle is the formation of multiple Er centres. We show that the previously identified cubic centre (Er-C) has C2v or lower…
Silicon films doped with Er and O were prepared by techniques of physical vapor deposition on crystalline silicon, ion beam mixing and oxygen incorporation through Ar+ and O2+ implantation, and thermal annealing. Processing steps were…
Here, we report the full-fledged journey towards the material synthesis and characterization of few-layered/thin WSe$_2$ using sputtered W-films on SiO$_2$/Si substrates followed by electrical studies under dark and illumination conditions.…
Recent progress achieved in metal-assisted chemical etching (MACE) has enabled the production of high-quality micropillar arrays for various optoelectronic applications. Si micropillars produced by MACE often show a porous Si/SiOx shell on…
At sub-Kelvin temperatures, two-level systems (TLS) present in amorphous dielectrics source a permittivity noise, degrading the performance of a wide range of devices using superconductive resonators such as qubits or kinetic inductance…
The relationship between the luminescence at 1.9 eV and the absorption bands at 2.0 eV and at 4.8 eV were investigated in a wide variety of synthetic silica samples exposed to different gamma- and beta-ray irradiation doses. We found that…
Si nanocrystals (Si-NC) in a-SiOx<Er> were created by high temperature annealing. Si-NC samples have large emission in a broadband region, 700nm to 1000nm. Annealing temperature, annealing time, substrate type, and erbium concentration is…