BFO3 ceramics were investigated by means of infrared reflectivity and time domain THz transmission spectroscopy at temperatures 20 - 950 K, and the magnetodielectric effect was studied at 10 - 300 K, with the magnetic field up to 9 T. Below…
We measured phonon dispersion in single crystal EuTiO$_3$ using inelastic x-ray scattering. A structural transition to an antiferrodistortive phase was found at a critical temperature $T_0$=287$\pm$1 K using powder and single-crystal x-ray…
Dielectric and magnetic properties of Eu0.5Ba0.25Sr0.25TiO3 are investigated between 10 K and 300 K in the frequency range from 10 Hz to 100 THz. A peak in permittivity revealed near 130 K and observed ferroelectric hysteresis loops prove…
Compressively strained epitaxial (001) EuTiO3 thin films of tetragonal symmetry have been deposited on (001) (LaAlO3)_0.29-(SrAl_{1/2}Ta_{1/2}O3)_0.71 (LSAT) substrates by reactive molecular-beam epitaxy. Enhancement of the Neel temperature…
The dielectric constant of the incipient ferroelectric EuTiO$_3$ exhibits a sharp decrease at about 5.5K, at which temperature antiferromagnetic ordering of the Eu spins simultaneously appears, indicating coupling between the magnetism and…
Polycrystalline ceramic samples and a single crystal of EuTiO3 have been investigated by Raman spectroscopy in the temperature range 80-300 K. Although synchrotron XRD data clearly indicated the cubic to tetragonal phase transition around…
We discuss the first infrared reflectivity measurement on a BiFeO3 single crystal between 5 K and room temperature. The 9 predicted ab-plane E phonon modes are fully and unambiguously determined. The frequencies of the 4 A1 c-axis phonons…
Hyper-Raman scattering experiments allowed collecting the spectra of the lowest F1u-symmetry mode of PbTiO3 crystal in the paraelectric phase up to 930K as well as down to about 1K above the phase transition. It is realized that this mode…
The magnetic susceptibility between 1.5 and 800 K, the infrared reflectivity at room temperature and the temperature dependence of the dielectric constant at mm-wavelengths are reported for single crystalline BiFeO3. A well developed…
We present a comprehensive study of polar and magnetic excitations in BiFeO3 ceramics and a thin film epitaxially grown on an orthorhombic (110) TbScO3 substrate. Infrared reflectivity spectroscopy was performed at temperatures from 5 to…
Here we report on an elastic and inelastic neutron scattering study addressing the effect of electric fields on quantum paraelectric SrTiO3. Our elastic scattering results find small changes as a function of field in a superlattice…
EuTiO3 (ETO) has recently experienced an enormous revival of interest because of its possible multiferroic properties which are currently in the focus of research. Unfortunately ETO is an unlikely candidate for enlarged multifunctionality…
EuTiO_3 is shown to exhibit novel strong spin-charge-lattice coupling deep in the paramagnetic phase. Its existence is evidenced by an, until now, unknown response of the paramagnetic susceptibility at temperatures exceeding the structural…
Ferroelectric soft mode properties in ceramics and thin films are reviewed and compared with single crystals. In general, the permittivity in ceramics and thin films is markedly reduced compared to the single crystals mainly because of…
X-ray diffraction, dynamical mechanical analysis and infrared reflectivity studies revealed an antiferrodistortive phase transition in EuTiO3 ceramics. Near 300K the perovskite structure changes from cubic Pm-3m to tetragonal I4/mcm due to…
Magnetic resonance spectra of EuTiO3 in both bulk and thin film form were taken at temperatures from 3-350 K and microwave frequencies from 9.2-9.8 and 34 GHz. In the paramagnetic phase, magnetic resonance spectra are determined by magnetic…
Polarized infrared reflectivity spectra of a (110)-oriented TbScO3 single crystal plate were measured down to 10 K. The number of observed polar phonons active along the crystallographic c axis at low temperatures is much higher than…
Infrared reflectivity spectra of cubic SrMnO$_{3}$ ceramics reveal 18 % stiffening of the lowest-frequency phonon below the antiferromagnetic phase transition occurring at T$_{N}$ = 233 K. Such a large temperature change of the polar phonon…
We provide a detailed study of the reflectivity of multiferroic TbMnO_3 for wave numbers from 40 cm^{-1} to 1000 cm^{-1} and temperatures 5 K < T < 300 K. Excitations are studied for polarization directions E || a, the polarization where…
Infrared reflection and transmission as a function of temperature have been measured on single crystals of Cu$_{3}$Bi(SeO$_{3}$)$_{2}$O$_{2}$Cl. The complex dielectric function and optical properties along all three principal axes of the…