Scratching the surface: Elastic rotations beneath nanoscratch and nanoindentation tests

Materials Science 2020-12-08 v2

Abstract

In this paper, we investigate the residual deformation field in the vicinity of nano-scratch tests using two orientations of a Berkovich tip on an (001) Cu single crystal. We compare the deformation with that from indentation, in an attempt to understand the mechanisms of deformation in tangential sliding. The lattice rotation fields are mapped experimentally using high-resolution electron backscatter diffraction (HR-EBSD) on cross-sections prepared using focused ion beam (FIB). A physically-based crystal plasticity finite element model (CPFEM) is used to simulate the lattice rotation fields, and provide insight into the 3D rotation field surrounding nano-scratch experiments, as it transitions from an initial static indentation to a steady-state scratch. The CPFEM simulations capture the experimental rotation fields with good fidelity, and show how the rotations about the scratch direction are reversed as the indenter moves away from the initial indentation.

Cite

@article{arxiv.2006.12554,
  title  = {Scratching the surface: Elastic rotations beneath nanoscratch and nanoindentation tests},
  author = {Anna Kareer and Edmund Tarleton and Christopher Hardie and Sarah V Hainsworth and Angus Wilkinson},
  journal= {arXiv preprint arXiv:2006.12554},
  year   = {2020}
}
R2 v1 2026-06-23T16:32:04.979Z