The fatigue fracture surfaces of a metallic alloy, and the stress corrosion fracture surfaces of glass are investigated as a function of crack velocity. It is shown that in both cases, there are two fracture regimes, which have a well defined self-affine signature. At high enough length scales, the universal roughness index 0.78 is recovered. At smaller length scales, the roughness exponent is close to 0.50. The crossover length ξc separating these two regimes strongly depends on the material, and exhibits a power-law decrease with the measured crack velocity ξc∝v−ϕ, with ϕ≃1. The exponents ν and β characterising the dependence of ξc and v upon the pulling force are shown to be close to ν≃2 and β≃2.
@article{arxiv.cond-mat/9610145,
title = {Pinning/depinning of crack fronts in heterogeneous materials},
author = {P. Daguier and B. Nghiem and E. Bouchaud and F. Creuzet},
journal= {arXiv preprint arXiv:cond-mat/9610145},
year = {2009}
}
Comments
4 pages, latex, and 4 encapsulated postscript figures