In the pursuit of developing high-temperature alloys with improved properties for meeting the performance requirements of next-generation energy and aerospace demands, integrated computational materials engineering (ICME) has played a crucial role. In this paper a machine learning (ML) approach is presented, capable of predicting the temperature-dependent yield strengths of superalloys, utilizing a bilinear log model. Importantly, the model introduces the parameter break temperature, Tbreak, which serves as an upper boundary for operating conditions, ensuring acceptable mechanical performance. In contrast to conventional black-box approaches, our model is based on the underlying fundamental physics, directly built into the model. We present a technique of global optimization, one allowing the concurrent optimization of model parameters over the low-temperature and high-temperature regimes. The results presented extend previous work on high-entropy alloys (HEAs) and offer further support for the bilinear log model and its applicability for modeling the temperature-dependent strength behavior of superalloys as well as HEAs.
@article{arxiv.2211.16576,
title = {Physics-Based Machine Learning Approach for Modeling the Temperature-Dependent Yield Strength of Superalloys},
author = {Baldur Steingrimsson and Xuesong Fan and Benjamin Adam and Peter K. Liaw},
journal= {arXiv preprint arXiv:2211.16576},
year = {2022}
}
Comments
arXiv admin note: text overlap with arXiv:2207.05171