English

Nanoindentation stress-strain for Fracture Analysis and computational modeling for hardness and modulus

Materials Science 2018-03-26 v1

Abstract

Stress-strain plots based on nanoindentation load-depth curves reflected cracking phenomenon. A transition from ductile to brittle fracture was observed on increasing the depth or load of indenter penetration. A new approach with shape factors in the fracture studies based on radial crack branching and micro-cracking was done. Hardness and modulus plots were fitted with polynomials. The coefficients were varied to obtain different hardness and modulus responses.

Keywords

Cite

@article{arxiv.1704.04525,
  title  = {Nanoindentation stress-strain for Fracture Analysis and computational modeling for hardness and modulus},
  author = {A. S. Bhattacharyya and S Priyadarshi and S. Sonu and S. Shivam and S. Anshu},
  journal= {arXiv preprint arXiv:1704.04525},
  year   = {2018}
}

Comments