Microstructure-property prediction of a Ni-based superalloy: A combined phase-field and finite element modelling approach

Materials Science 2023-10-10 v1

Abstract

Multiscale modelling is a new paradigm that has emerged in recent times to study the well-known problem of the process-structure-property relationship in the area of materials science and engineering. For obtaining the desired performance for materials of strategic importance, such as superalloys, it is essential to bridge different length and time scales in order to navigate the entire design space. In the present study, we develop a physics-based model for a Ni-based superalloy where the microstructures simulated using a phase-field model serve as input to finite-element computations. We examine the alloy's microstructure evolution and effective elastic properties quantitatively via phase-field and finite element methods integrated with CALPHAD database, by varying composition and aging temperature. The phase-field simulations provide us with an insight into the different regimes of microstructure evolution. The finite element analysis uncovers the relation of effective elastic properties with several system parameters.

Keywords

Cite

@article{arxiv.2310.04885,
  title  = {Microstructure-property prediction of a Ni-based superalloy: A combined phase-field and finite element modelling approach},
  author = {Rupesh Chafle and Vishal Panwar and Kaushik Das and Somnath Bhowmick and Rajdip Mukherjee},
  journal= {arXiv preprint arXiv:2310.04885},
  year   = {2023}
}