Evidence for hydrogen two-level systems in atomic layer deposition oxides

Materials Science 2015-03-19 v1 Superconductivity

Abstract

Two-level system (TLS) defects in dielectrics are known to limit the performance of electronic devices. We study TLS using millikelvin microwave loss measurements of three atomic layer deposited (ALD) oxide films--crystalline BeO (cBeO\rm{c-BeO}), amorphous Al2O3\rm{Al_2O_3} (aAl2O3\rm{a-Al_2O_3}), and amorphous LaAlO3\rm{LaAlO_3} (aLaAlO3\rm{a-LaAlO_3})--and interpret them with room temperature characterization measurements. We find that the bulk loss tangent in the crystalline film is 6 times higher than in the amorphous films. In addition, its power saturation agrees with an amorphous distribution of TLS. Through a comparison of loss tangent data to secondary ion mass spectrometry (SIMS) impurity analysis we find that the dominant loss in all film types is consistent with hydrogen-based TLS. In the amorphous films excess hydrogen is found at the ambient-exposed surface, and we extract the associated hydrogen-based surface loss tangent. Data from films with a factor of 40 difference in carbon impurities revealed that carbon is currently a negligible contributor to TLS loss.

Keywords

Cite

@article{arxiv.1307.7664,
  title  = {Evidence for hydrogen two-level systems in atomic layer deposition oxides},
  author = {M. S. Khalil and M. J. A. Stoutimore and S. Gladchenko and A. M. Holder and C. B. Musgrave and A. C. Kozen and G. Rubloff and Y. Q. Liu and R. G. Gordon and J. H. Yum and S. K. Banerjee and C. J. Lobb and K. D. Osborn},
  journal= {arXiv preprint arXiv:1307.7664},
  year   = {2015}
}

Comments

11 pages, 4 figures (preprint format)

R2 v1 2026-06-22T00:59:44.544Z