Atomic layer deposition and superconducting properties of NbSi films

Materials Science 2011-04-19 v1 Instrumentation and Methods for Astrophysics

Abstract

Atomic layer deposition was used to synthesize niobium silicide (NbSi) films with a 1:1 stoichiometry, using NbF5 and Si2H6 as precursors. The growth mechanism at 200oC was examined by in-situ quartz crystal microbalance (QCM) and quadrupole mass spectrometer (QMS). This study revealed a self-limiting reaction with a growth rate of 4.5 {\AA}/cycle. NbSi was found to grow only on oxide-free films prepared using halogenated precursors. The electronic properties, growth rate, chemical composition, and structure of the films were studied over the deposition temperature range 150-400oC. For all temperatures, the films are found to be stoichiometric NbSi (1:1) with no detectable fluorine impurities, amorphous with a density of 6.65g/cm3, and metallic with a resistivity {\rho}=150 {\mu}{\Omega}.cm at 300K for films thicker than 35 nm. The growth rate was nearly constant for deposition temperatures between 150-275oC, but increases above 300oC suggesting the onset of non-self limiting growth. The electronic properties of the films were measured down to 1.2K and revealed a superconducting transition at Tc=3.1K. To our knowledge, a superconducting niobium silicide film with a 1:1 stoichiometry has never been grown before by any technique.

Keywords

Cite

@article{arxiv.1104.3518,
  title  = {Atomic layer deposition and superconducting properties of NbSi films},
  author = {Thomas Proslier and Jeffrey A. Klug and Jeffrey W. Elam and Helmut Claus and Nicholas G. Becker and Michael Pellin},
  journal= {arXiv preprint arXiv:1104.3518},
  year   = {2011}
}

Comments

9 figures, ~ 10 pages. Poster Jeffrey Klug @ ALD conference 2010